Technical information
| Description | Thick × Wide [mm×mm] | Sectional area [mm2] | Weight [g/m] | Expansion of tape × 10(-4) [/N] | Young's modulus × 104 [N/mm2] | Coefficient expansion × 10(-6) [/°C] | 
|---|---|---|---|---|---|---|
| Stilon Tape Yeron Tape | 0.13 × 10 | 1.27 ± 1% | 14.6 ± 1% | 0.0383 | 20.58 | 11.5 | 
| Silver Tape | 0.19 × 13 | 2.52 ± 1% | 19.8 ± 1.5% | 0.0196 | 20.29 | 11.5 | 
Remarks: Thick × Wide and Sectional area show only padding and the weight contains the coated nylon and paint.
FORMULA OF CORRECTIONS:
- Temperature correction formula: La(T-20) = Ct
- Tension correction formula: (Expansion) × (P - Po)L = Cp
- Looseness correction formula: {(mg)2 × L3}/(24P2) = {(Mg)2 × L}/(24P2) = -Cs
- Ct: Value after temperature correction
- Cp: Value after tension correction
- -Cs: Value after looseness correction
Note:
- T :
- Temperature at time of measurement [°C]
- P :
- Tension at time of measurement [N]
- Po :
- Tension of tape [N]
- L :
- Length on tape [mm]
- m :
- Weight per unit of length of tape [kg/m]
- M :
- Weight of tape supported between two measuring points [kg]
- a :
- Coefficient of linear expansion of tape [/°C]
- g :
- Acceleration of gravity 9.80665 m/(s2)]
Specifications may be changed for improvement without notice.